EN
Troubleshooting

How to fix stringing in 3D prints

Those cobweb-like strings between two parts of a print appear when plastic oozes while the nozzle travels without printing. Here is how to get rid of them, from the simplest fix to the finest tuning.

NFC3D · 27 November 2026 · 5 min read

1. Dry the filament

Before touching any setting, rule out moisture. Wet filament turns into steam inside the nozzle, which pushes plastic out even after the printer retracts. Typical signs: popping while printing, bubbles and a rough surface. PETG and TPU suffer the most. If that is your case, dry it (the guide PLA vs PETG vs TPU has typical temperatures) and test again.

2. Lower the nozzle temperature

The hotter it is, the runnier the plastic and the more it oozes. Go down in 5 °C steps without leaving the range given by the maker. The easiest way is a temperature tower: a single part printed while the temperature changes every few millimetres. OrcaSlicer has one in its calibration menu.

Do not go so low that layers stop bonding: if the part snaps easily between layers, you went too far.

3. Tune retraction

Retraction pulls the filament back before each travel move so it does not ooze. There are two values:

Too much retraction is also bad: it can cause jams or gaps at the start of each line. Change one value at a time in small steps; modern slicers also include a retraction test in the calibration menu.

4. Less travel through the air

5. More fan

With PLA, a part-cooling fan at full speed cools the string sooner so it breaks. With PETG, do not overdo it: too much fan weakens layer bonding.

If a few remain

A couple of loose strings disappear in seconds with a lighter or a heat gun passed quickly, without getting too close. If there are many, go back to step 1.