PLA vs PETG vs TPU: which filament to use for each part
The three most common filaments for home printers are good at different things. Picking the right one saves you broken, warped or unstuck prints.
At a glance
| PLA | PETG | TPU | |
|---|---|---|---|
| Ease | Very easy | Easy | Medium |
| Stiffness | High, but brittle | Medium, impact resistant | Flexible, rubber-like |
| Heat | Softens around 55–60 °C | Up to about 70–80 °C | Depends on hardness |
| Typical use | Figures, prototypes, decor | Functional parts, outdoors, car | Cases, bumpers, gaskets |
Temperatures in this article are a guide only. Always follow what the filament maker prints on the box or website.
PLA: the starting point
It is the easiest to print, comes in the most colours and finishes (silk, matte, wood, glitter) and warps the least. It is usually printed at 190–220 °C with the bed at 50–60 °C.
- Pros: fine detail, good accuracy, almost no smell, ideal for multicolour.
- Cons: brittle under impact and softens with little heat. A PLA part left in a car in the summer sun can bend.
PETG: when the part has a job to do
It is tougher than PLA: instead of snapping, it gives a little. It handles heat, sunlight and moisture better, which makes it a good choice for brackets, outdoor parts, everyday keychains and anything that lives in the car. It is usually printed at 220–250 °C with the bed at 70–85 °C.
- Strings: it tends to leave fine strings between parts. Tuning retraction and drying the filament help a lot (see how to fix stringing).
- Sticks too well to some smooth PEI or glass beds. A thin layer of glue stick acts as a release agent and stops it tearing bits off the surface.
- Print a little slower than PLA and with less fan so layers bond properly.
TPU: flexible parts
TPU is an elastic plastic. Its hardness is given in Shore (95A is the most common for home printing; the lower the number, the softer). It is used for phone cases, wheels, bumpers, gaskets and straps.
- Slowly: it is printed slowly, often at 15–40 mm/s, because the filament compresses inside the extruder.
- Direct drive: it works much better with a direct-drive extruder than with a long Bowden tube.
- Multicolour: many automatic multicolour systems do not accept flexible filament. Check your printer's manual before loading it.
- Reduce or disable retraction if you get jams.
Moisture ruins everything
All these plastics absorb water from the air, some more than others (TPU and PETG quite a lot). Wet filament pops and crackles at the nozzle, leaves strings, bubbles and rough surfaces, and makes weaker parts.
- Store spools in sealed bags or boxes with silica gel packs.
- If it has already absorbed moisture, dry it in a filament dryer or an oven that holds low temperatures accurately. As a guide, PLA dries at about 45–55 °C and PETG and TPU at about 55–65 °C, for several hours.
- Do not overdo the temperature: PLA softens and the spool can stick together.
What about a keychain?
PLA for gifts and keychains that live in a drawer or a backpack. PETG for everyday or car keys. The guide how to design a keychain that will not break has the measurements, and the keychain generator lets you choose PLA, PETG or TPU when you download the file.